TM 10-5411-207-14
4-7.
Delamination Repair (cont).
(k) Grind repaired surface smooth and using emery cloth or sandpaper,
remove any rough areas on surface and thoroughly clean repaired area
with a soft cloth lightly coated with alcohol or toluene.
(l)
Prime and paint repaired panel surface and heads of pop rivets. (Refer to
paragraph 4-12.)